Journal: :Journal of Japan Institute of Light Metals 1993

2015
Radosław Łyszkowski

The isothermal oxidation of Fe-28Al-5Cr (at%) intermetallic alloy microalloyed with Zr and B (<0.08 at%) in air atmosphere, in the temperature range of 1000 to 1200 °C, was studied. The investigation was carried out on the thin-walled (<1 mm) elements prepared by Laser Engineered Net Shaping (LENS) from alloy powder of a given composition. Characterization of the specimens, after the oxidation,...

2015
A. Ojha S. Alkan L. Patriarca H. Sehitoglu

The Fe3Al alloy with D03 structure exhibits large recoverable strains due to reversible slips. Tension and compression experiments were conducted on single crystals of Fe3Al, and the onset of slip in forward and reverse directions were obtained utilizing high-resolution digital image correlation technique. The back stress provides the driving force for reversal of deformation upon unloading, re...

نمودار تعداد نتایج جستجو در هر سال

با کلیک روی نمودار نتایج را به سال انتشار فیلتر کنید