نتایج جستجو برای: wear debris and microstructure examination
تعداد نتایج: 16859548 فیلتر نتایج به سال:
in this research, surface composite layers containing nano sized tib2, al2o3-tib2, zro2 and cnt particles have been fabricated on aluminum alloy substrates by friction stir processing. the effects of different processing variables such as number of passes and strengthening particle distribution, hardness, and wear properties of surface nanocomposite layers have been evaluated by electron micros...
Wear debris, of deferent sizes, shapes and quantities, generated in artificial hip and knees is largely confined to the bone and joint interface. This debris interacts with periprosthetic tissue and may cause aseptic loosening. The purpose of this review is to summarize and collate findings of the recent demonstrations on debris characterization and their biological response that influences the...
Twenty-four clinically successful, autopsy retrieved porous-coated anatomic total knee arthroplasty (TKA) specimens were evaluated to determine the structure and function of the patellar meniscus. Mean implant duration was 76 months (range: 11-135 months). Histological examination showed the patellar meniscus to be composed of dense fibrous tissue with scattered regions of chronic granulomatous...
Periprosthetic osteolysis is the most common long-term complication of a total joint arthroplasty, often resulting in aseptic loosening of the implant, which occurs in up to 34% of younger implant recipients and usually requires surgical revision. Particulate wear debris, continuously generated by articulating motion at the bearing surfaces, has been implicated as one of the primary causes of p...
The long-term success of a total joint replacement can be undermined by loosening of the implant, generation of wear debris or a combination of both factors. In the present study the influence of the surface morphologies of the bone and cement mantle on loosening of cemented total joint replacements (THJRs) and development of wear debris were studied. Model cemented THJR specimens were prepared...
Ti-6Al-4V titanium alloy has great application in medicine and military industries due to its capabilities, namely high strength to weight ratio and corrosion resistance. In the current research, the effect of aging treatment on microstructure and wear behavior of Ti-6Al-4V titanium alloy was investigated. Pin on disk wear test was applied to assess the wear behavior. Specimens were first solut...
The biological significance of cobalt-chromium wear particles from metal-on-metal hip replacements may be different to the effects of the constituent metal ions in solution. Bacteria may be able to discriminate between particulate and ionic forms of these metals because of a transmembrane nickel/cobalt-permease. It is not known whether wear particles are bacteriocidal. We compared the doubling ...
The average life span of knee prosthesis used in Total Knee Replacement (TKR) is approximately 10 to 15 years. Literature indicates that the reasons for implant failures include wear, infection, instability, and stiffness. However, the majority of failures are due to wear and tear of the prosthesis. The most common biopolymer used in TKR is Ultra High Molecular Weight Polyethylene (UHMWPE). Pr...
Wear debris-induced osteolysis remains the greatest limitation of long-term success for total joint replacements with ultra-high molecular weight polyethylene (UHMWPE) bearings. To address oxidative degradation post-gamma irradiation, manufacturers are investigating the incorporation of antioxidants into PE resins. Similarly, larger molecular weight monomers have been developed to increase cros...
نمودار تعداد نتایج جستجو در هر سال
با کلیک روی نمودار نتایج را به سال انتشار فیلتر کنید