نتایج جستجو برای: stand off distance

تعداد نتایج: 450434  

ژورنال: مواد پرانرژی 2018

In the present research, the influences of explosive welding parameters on the corrosion behavior of the three layer explosive welds of the tubes Al 5083 / Al 1050 / stcr18Ni9Ti in the salt environment was investigated. The selected parameters included the stand-off distance and the thickness of the explosive charge. Therefore, two samples A and B were welded with stand-off distances of 6 and 6...

Journal: Polyolefins Journal 2020

Polyamide 6 / nitrile butadiene rubber / nanoclay (PA6/NBR/clay) nanocomposite has gathered wide acceptance in industry. Laser welding, as a fabrication method, is applied to welding of polymer nanocomposites. In this study, the input parameters (clay (Closite 30B) content, laser power, scan velocity and stand-off-distance) are varied to achieve the best responses (tensile strength of welds). R...

ژورنال: مواد پرانرژی 2020

In the present study, the effect of explosive welding stand-off distance on the structure and corrosion behavior of aluminum alloy 5083-copper joint is studied. The microstructure was examined by optical microscopy and scanning electron microscopy and corrosion behavior with poteniodynamic polarization tests and electrochemical impedance spectroscopy in a salt environment. Microscopic results s...

ژورنال: مواد پرانرژی 2022

In the current research, the microstructural changes and corrosion behavior of two-layer Steel/Bronze sheets were investigated after the heat treatment of the explosive welding process. The heat treatment was performed at 600ºC for 16 hr. Dynamic potential polarization, electrochemical impedance spectroscopy, optical microscopy, and scanning electron microscopy analyses were used. Based on of t...

ژورنال: مواد پرانرژی 2019

In this research, the effect of the amount of strain and rolling temperature on the microstructure and the hardness of the explosive bonding of 304 stainless steel- copper sheets was investigated. Explosive welding was performed with two explosive thickness (46 and 79 mm) and stand-off distance (2 and 3 mm). The results of the optical microscope after welding showed that all samples had a commo...

2013
Wei Xie James Wang Christopher C. Berndt

A single splat is the building block of a thermal spray coating; thus, investigating single splats is essential to understanding thermal spray coatings and their properties. In this study, the morphology of flame sprayed ethylene methacrylic acid (EMAA) splats, deposited at various stand-off distances (SODs) onto glass and mild steel substrates were investigated using a scanning electron micros...

2015
Gaurav Upadhyay Kamal Hassan

Stainlesssteel 403 is high-alloysteelwith good corrosion resistance and it’svery hard material. Abrasive water jet is an effective method for machining, cutting and drilling of stainlesssteel 403. In thispaperweoptimize the metalremoval rate of stainlesssteel 403 in abrasive water jet machining. The MRRisoptimize by usingthreeparameters water pressure, abrasive flow rate and stand-off distance ...

Journal: :journal of computational applied mechanics 0
amirhossein bayat university of zanjan rasoul moharami assistant professor of engineering department, university of zanjan

structural health monitoring of cracked structures is one of beloved subject of researchers recently. consider of crack behavior in the water and energy pipeline is important because of environmental problems. in this paper consider of crack parameters in the underwater pipe subjected to mechanical transient load is investigated. for this purpose, three- dimensional parametric model of cracked ...

Journal: :Index on Censorship 2015

نمودار تعداد نتایج جستجو در هر سال

با کلیک روی نمودار نتایج را به سال انتشار فیلتر کنید