Study the Profile Shape and Mechanical Properties of Bonded Joint HNV3 to Nimonic 80A Superalloy with Inertia Friction Welding Method

نویسندگان

  • Abbasi , M.
  • Sakiyan, S.
چکیده مقاله:

This Paper presents the welding parameterchr('39')s effect (forging pressure, welding time) on macrostructure and mechanical properties of friction welding valve steel HNV3 to Nimonic 80A super alloy. For this purpose, two rods with 20 mm diameters are prepared and with using different parameters (Increase forging pressure and welding time) by friction welding method are welded together. Tensile Test carried out on samples for investigating the effect of a parameter. It was discovered that when the welding parameters used in connecting HNV3 and Nimonic 80A Superalloy couple through friction welding were selected correctly; strength of the connection would increase compared to the main material.

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Prediction of the Hot Compressive Deformation Behavior for Superalloy Nimonic 80A by BP-ANN Model

Abstract: In order to predict hot deformation behavior of superalloy nimonic 80A, a back-propagational artificial neural network (BP-ANN) and strain-dependent Arrhenius-type model were established based on the experimental data from isothermal compression tests on a Gleeble-3500 thermo-mechanical simulator at temperatures ranging of 1050–1250 ̋C, strain rates ranging of 0.01–10.0 s ́1. A comparis...

متن کامل

determination of some physical and mechanical properties red bean

چکیده: در این تحقیق، برخی خواص فیزیکی و مکانیکی لوبیا قرمز به-صورت تابعی از محتوی رطوبت بررسی شد. نتایج نشان داد که رطوبت بر خواص فیزیکی لوبیا قرمز شامل طول، عرض، ضخامت، قطر متوسط هندسی، قطر متوسط حسابی، سطح تصویر شده، حجم، چگالی توده، تخلخل، وزن هزار دانه و زاویه ی استقرار استاتیکی در سطح احتمال 1 درصد اثر معنی داری دارد. به طوری که با افزایش رطوبت از 54/7 به 12 درصد بر پایه خشک طول، عرض، ضخام...

15 صفحه اول

Microstructure and Mechanical Properties of the Friction Welded Joint between X53CrMnNiN219 and X45CrSi93 Stainless Steel

Dissimilar metals friction welding of austenitic–martensitic stainless steels is commonly used in order to manufacture engine valves in the automobile industry. In this study, X53CrMnNiN219 (austenitic stainless steel) and X45CrSi93 (martensitic stainless steel) valve steel rods were welded by friction welding process. The welded joint was then heat treated at 760 0C for 60 min. Mechanical prop...

متن کامل

Effect of Laser Spot Welding Variables on Microstructure and Mechanical Properties of the Ti-6AL-4V to AISI304 Dissimilar Joint

In this project, joining Ti-6Al-4V and AISI 304 dissimilar plates by laser-spot-welding method has been studied. In this regard, Ti-6Al-4V and AISI 304 plates, with a thickness of 0.7 and 0.5 respectively, were lap-welded using an interlayer of 0.2 & 0.3 mm copper and silver (pure silver). The process was done by 400Watt pulsed laser (Nd:YAG) using oncentric spot welding with 4mm diameter circl...

متن کامل

Effect of Laser Spot Welding Variables on Microstructure and Mechanical Properties of the Ti-6AL-4V to AISI304 Dissimilar Joint

In this project, joining Ti-6Al-4V and AISI 304 dissimilar plates by laser-spot-welding method has been studied. In this regard, Ti-6Al-4V and AISI 304 plates, with a thickness of 0.7 and 0.5 respectively, were lap-welded using an interlayer of 0.2 & 0.3 mm copper and silver (pure silver). The process was done by 400Watt pulsed laser (Nd:YAG) using oncentric spot welding with 4mm diameter circl...

متن کامل

منابع من

با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ذخیره در منابع من قبلا به منابع من ذحیره شده

{@ msg_add @}


عنوان ژورنال

دوره 2  شماره 1

صفحات  14- 20

تاریخ انتشار 2016-08

با دنبال کردن یک ژورنال هنگامی که شماره جدید این ژورنال منتشر می شود به شما از طریق ایمیل اطلاع داده می شود.

کلمات کلیدی

کلمات کلیدی برای این مقاله ارائه نشده است

میزبانی شده توسط پلتفرم ابری doprax.com

copyright © 2015-2023