Microstructure of spark plasma sintered TiB2 and TiB2–AlN ceramics

نویسندگان

  • Mehdi Shahedi Asl Department of Mechanical Engineering, University of Mohaghegh Ardabili, Ardabil, Iran
  • Zohre Ahmadi Ceramic Department, Materials and Energy Research Center (MERC), Karaj, Iran
چکیده مقاله:

In this research study, the effects of aluminum nitride (AlN) additive on the densification behavior and microstructure development of titanium diboride (TiB2) based ceramic matrix composite were investigated. In this way, a monolithic TiB2 ceramic and a TiB2–5 wt% AlN ultrahigh temperature ceramic composite were fabricated by spark plasma sintering (SPS) process at a temperature of 1900 °C for a dwell time of 7 min under an externally applied pressure of 40 MPa in vacuum conditions. The relative density measurements were carried out using the Archimedes principles for evaluation of bulk density and rule of mixtures for calculation of theoretical one. Compared to the additive-free monolithic TiB2 ceramic sample with a relative density of ~96%, the addition of AlN as a sintering aid greatly improved the sinterability of TiB2 matrix composite so that a near fully dense sample with a relative density of ~100% were obtained by the spark plasma sintering process. The removal of harmful oxide impurities of titania (TiO2) and boria (B2O3) from the surfaces of starting TiB2 powder particles and in-situ formation of new phases such as aluminum diboride (AlB2) and Al2Ti as an intermetallic compound of aluminum and titanium, not only improved the sinterability of the composite ceramic, but also significantly prevented the extreme growth of TiB2 grains.

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Microstructure and Properties of Spark Plasma Sintered MoAlB Ceramics

Advisor: Bai Cui Molybdenum aluminum boride (MoAlB) is a ternary transition metal boride which has promising aeronautic and nuclear applications. It inheres excellent properties of the binary transitional metal borides (e.g., MoB, ZrB2) such as high melting temperature, high hardness, and thermal conductivity. Besides, MoAlB is superior to MoB because: (1) the Al element provides an oxidation r...

متن کامل

Microstructure of Spark Plasma-Sintered Silicon Nitride Ceramics

The microstructure and phase composition of the high-content Al2O3-Y2O3-doped spark plasma-sintered silicon nitride were investigated. Fully dense silicon nitride ceramics with a typical α-Si3N4 equiaxed structure with average grain size from 200 to 530 nm, high elastic modulus of 288 GPa, and high hardness of 2038 HV were spark plasma sintered (SPSed) at 1550 °C. Silicon nitride with elongated...

متن کامل

Phase assembly and electrical conductivity of spark plasma 4 sintered CeO 2 – ZrO 2 ceramics 5

10 Abstract CexZr1-xO2 (x = 0.10, 0.16 and 0.33) nano11 crystalline powders were obtained by a two-step synthesis 12 technique and sintered by spark plasma sintering (SPS). As 13 consequence of the reduction of Ce to Ce species by 14 carbon in the graphite environment in SPS, phase assem15 blies including tetragonal, monoclinic and pyrochlore 16 phases were generated in the ceramics during the ...

متن کامل

Microstructure and Properties of Spark Plasma Sintered Aluminum Containing 1 wt.% SiC Nanoparticles

The low hardness and strength of aluminum, which limits its use in many industrial applications, could be increased through the addition of nanoparticles. However, the appropriate processing method and parameters should be carefully selected in order to achieve the desired improvement in properties. In this work, aluminum was reinforced with low weight fraction (1 wt.%) of SiC nanoparticles and...

متن کامل

Biomimetic apatite sintered at very low temperature by spark plasma sintering: physico-chemistry and microstructure aspects.

Nanocrystalline apatites analogous to bone mineral are very promising materials for the preparation of highly bioactive ceramics due to their unique intrinsic physico-chemical characteristics. Their surface reactivity is indeed linked to the presence of a metastable hydrated layer on the surface of the nanocrystals. Yet the sintering of such apatites by conventional techniques, at high temperat...

متن کامل

Grain growth kinetic of spark plasma sintered magnesia

In this research, the densification of magnesia nanopowder with a mean particle size of about 100 nm was investigated by spark plasma sintering undera pressures of 80 MPa and at temperature range from 1000 °C to 1400 °C and a heating rate of 50 °C/min for 20 minutes. The density of the samples slowly increased with increasing sintering temperatures to 1200 °C. Afterwards, with more increasing o...

متن کامل

منابع من

با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ذخیره در منابع من قبلا به منابع من ذحیره شده

{@ msg_add @}


عنوان ژورنال

دوره 5  شماره 1

صفحات  36- 40

تاریخ انتشار 2019-03-01