Nickel Base Superalloy Rene®80 – The Effect of High Temperature Cyclic Oxidation on Platinum-Aluminide Coating Features

نویسندگان

  • K. Shirvani Department of Advanced Materials and New Energies, Iranian Research organization for Science and Technology (IROST), Tehran, Iran
  • K. Zangeneh madar Metallic Materials Research Center, Malek Ashtar University of Technology (MUT), Tehran, Iran
  • M.M. Barjesteh Metallic Materials Research Center, Malek Ashtar University of Technology (MUT), Tehran, Iran
  • S. M.i Abbasi Metallic Materials Research Center, Malek Ashtar University of Technology (MUT), Tehran, Iran
چکیده مقاله:

Nickel base superalloy alloys are used in the manufacture of gas turbine engine components, which in use are exposed to high temperatures and corrosive environments. The platinum aluminide coatings described here have been developed to protect nickel base superalloy alloys from oxidation. In this study, the effect of cyclic oxidation, platinum layer thickness and aluminizing process on behavior of Pt-Aluminide (Pt-Al) coating on nickel-based superalloy Rene®80 have been investigated. For this purpose, after applying different thicknesses of Pt-layer (2, 6 and 8µm), diffusion aluminide coating in two types, high temperature-low activity (HTLA) and low temperature-high activity (LTHA) methods was performed. The results of microstructural investigations by Scanning Electron Microscopy and the X-ray diffraction analysis indicated that coatings include three zones in all thicknesses of the platinum layer and in both methods of aluminizing. The results of cyclic oxidation (1100 °C and 120 cycles) test showed that Pt-Al in all conditions improved the oxidation resistance of Rene®80. The best oxidation resistance is related to the specimen coated with 6 µm Pt by LTHA method, whereas the lowest resistance was related to 2µm Pt in the case of HTLA method. The weight changes during cyclic oxidation of 6µm Pt (LTHA) and 2µm Pt (HTLA) coatings were 3.8 and 6 mg, respectively. Also, the parabolic oxidation rate constants of these coatings were calculated as 1.5*10-12 and 3.8*10-12, respectively.

Download for Free

Sign up for free to access the full text

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Cyclic oxidation-induced cracking of platinum-modified nickel-aluminide coatings

Short cracks, extending to the interdiffusion zone, have been observed in platinum-modified nickel-aluminide diffusion coatings on single-crystal CMSX-4 superalloys after these have been subject to short (10 min) rapid thermal cycles. The cracks were revealed after removing the thermally grown oxide formed during cycling on the coating surfaces. Cracking was observed for coatings subject to the...

متن کامل

Cyclic oxidation behavior of uncoated and aluminum-rich nickel aluminide coated Rene-80 superalloy

In this study, aluminide coating was employed to enhance the high-temperature cyclic oxidation of Rene-80 superalloy at 950ºC. The microstructural aspects and phase constituents of samples were  investigated with scanning electron microscopy (SEM) and x-ray diffraction (XRD) techniques. The result of oxidation tests showed that the weight gain in the uncoated sample was considerably higher than...

متن کامل

On the initiation of cyclic oxidation-induced rumpling of platinum-modified nickel aluminide coatings

The evolution of the surface roughness of an initially flat platinum-modified nickel aluminide (NiPtAl) coating on a single crystal superalloy with cyclic oxidation has been measured by optical profilometry and correlated with the aluminide microstructure. The roughness evolution is dominated by the relative motion of individual grains on thermal cycling, with the larger sized grains moving up ...

متن کامل

Formation Mechanism of Silicon Modified Aluminide Coating on a Ni-Base Superalloy

Formation mechanism of silicon modified aluminide coating applied on a nickel base super alloy IN-738 LC by pack cementation process was the subject of investigation in this research. Study of the microstructure and compositions of the coating was carried out, using optical and scanning electron microscopes, EDS and X-ray diffraction (XRD) techniques. The results showed that due to low partial ...

متن کامل

Formation and Evaluation of Oxidation Behavior of Zirconia- Aluminide Coating on Nickel- Based Alloy

Practical applications of thermal barrier coatings with aluminide bond-coats are limited due to oxide scale spallation of the aluminide coating under applied thermal stresses. Considering the positive effects of oxygen-active elements or their oxides on the high temperature oxidation behavior, in this research zirconia was introduced into an aluminide coating. For this purpose, a Watts type bat...

متن کامل

High Temperature Oxidation Performance of Aluminide Coatings

In order to determine the potential benefits and limitations of aluminide coatings, coatings made by chemical vapor deposition (CVD) on Feand Ni-base alloy substrates are being evaluated in various hightemperature environments. Testing of coatings on representative ferritic (Fe-9Cr-1Mo) and austenitic (type 304L stainless steel) alloys has found that high frequency thermal cycling (1h cycle tim...

متن کامل

منابع من

با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ذخیره در منابع من قبلا به منابع من ذحیره شده

{@ msg_add @}


عنوان ژورنال

دوره 13  شماره 1

صفحات  11- 22

تاریخ انتشار 2020-02-01

با دنبال کردن یک ژورنال هنگامی که شماره جدید این ژورنال منتشر می شود به شما از طریق ایمیل اطلاع داده می شود.

میزبانی شده توسط پلتفرم ابری doprax.com

copyright © 2015-2023