In this study, the effect of Ta/W ratio on the microstructure and stress rupture properties of Ni-based single crystal (SX) superalloy PWA1483 was investigated. For this purpose, single crystal (SX) superalloys with different Ta/W ratios (0.75, 1.0, 1.32 and 1.5 in wt.%) were fabricated. The alloys were directionally solidified by Bridgman method under the same solidification condition at withd...

It is well-known that the harsh operational conditions of turbine blades lead to a gradual change in the microstructure of underlying Ni-based superalloy of blades. According to this, a rejuvenation process should be conducted on turbine blades superalloys to recover their microstructures. The first and main step of rejuvenation process is the determination of appropriate solution condition in ...

2018
Liming Tan Guoai He Feng Liu Yunping Li Liang Jiang

The microstructure with homogeneously distributed grains and less prior particle boundary (PPB) precipitates is always desired for powder metallurgy superalloys after hot isostatic pressing (HIPping). In this work, we studied the effects of HIPping parameters, temperature and pressure on the grain structure in PM superalloy FGH96, by means of scanning electron microscope (SEM), electron backsca...

2010
Andrzej Nowotnik Jan Sieniawski

Experimental results on hot deformation and dynamic structural processes of nickel based alloy Inconel 718 are reviewed. The focus is the analysis of dynamic precipitation processes which operate during hot deformation of these materials at elevated temperatures. Hot compression tests were performed on the solution treated precipitation hardenable nickel based superalloy Inconel 718 at 720-1150...

Journal: :International journal of advanced research 2021

The creep of the pre-strained superalloy N07080 is described in this work. pre-strain was achieved by warm rolling at 1050 oC.-The performed due to additional strengthening, i.e increasing hardness.-The drastically reduces rupture life compared standard heat treated superalloy.-The drastic reductionof result rapid cavity nucleation on stress concentration sites along primary grain boundaries su...

Behrooz Movahedi, Iraj Lirabi Mehdi Bazargan Rasool Mokhtari Homami

In this paper, the performance of the cutting tool with nanocrystalline multilayer coatings (TiN+TiAlN) for machining of superalloy Inconel 718 in the dry and wet conditions was studied. The multi layer TiN and TiAlN with nanocrystalline structure was applied by physical vapor deposition technique (arc evaporation) on the WC-Co inserts. The results of the ball on disc wear test and the machinin...

Nickel base superalloy alloys are used in the manufacture of gas turbine engine components, which in use are exposed to high temperatures and corrosive environments. The platinum aluminide coatings described here have been developed to protect nickel base superalloy alloys from oxidation. In this study, the effect of cyclic oxidation, platinum layer thickness and aluminizing process on beha...

Journal: :international journal of advanced design and manufacturing technology 0
mojtaba kolahdoozan department of mechanical engineering, najafabad branch, islamic azad university, isfahan, iran farhad azimifar department of mechanical engineering, majlesi branch, islamic azad university, isfahan, iran saeed rismani yazdi department of mechanical engineering, majlesi branch, islamic azad university, isfahan, iran

in this research, our attempt is to monitor tool wear through the chip formations, forces, and temperature of edge of drill while drilling in superalloy plate to optimizes effective parameters, which lead to facilitate machining process to, improved tool life, and enhance the productivity. in this study, inconel718 superalloy material, and cemented coated carbide tool was selected for investiga...

2003
D. S. Balint J. W. Hutchinson

Undulation instabilities in a tri-layer system subject to variations of temperature are studied for the purpose of revealing a mechanism leading to the failure of thermal barrier systems. A pre-compressed oxide film with a small initial non-planarity is attached to a metal bond coat layer that is, in turn, attached to a thick superalloy substrate. The oxide film and the superalloy substrate are...